通过深冷轧制和短时低温退火实现纯镍的高强度和拉伸延展性

a Light Alloys Research Institute, Central South University, Changsha 410083, China
b State Key Laboratory of High Performance Complex Manufacturing, Central South University, Changsha 410083, China
c College of Mechanical and Electrical Engineering, Central South University, Changsha 410083, China
d Electron Microscope Unit, University of New South Wales, Sydney, NSW 2052, Australia

发布日期: 2023-08-19

下一篇 上一篇

摘要

Ultrafine-grained pure metals and their alloys have high strength and low ductility. In this study, cryorolling under different strains followed by low-temperature short-time annealing was used to fabricate pure nickel sheets combining high strength with good ductility. The results show that, for different cryorolling strains, the uniform elongation was greatly increased without sacrificing the strength after annealing. A yield strength of 607 MPa and a uniform elongation of 11.7% were obtained after annealing at a small cryorolling strain (ε = 0.22), while annealing at a large cryorolling strain (ε = 1.6) resulted in a yield strength of 990 MPa and a uniform elongation of 6.4%. X-ray diffraction (XRD), transmission electron microscopy (TEM), scanning electron microscopy (SEM), and electron backscattered diffraction (EBSD) were used to characterize the microstructure of the specimens and showed that the high strength could be attributed to strain hardening during cryorolling, with an additional contribution from grain refinement and the formation of dislocation walls. The high ductility could be attributed to annealing twins and micro-shear bands during stretching, which improved the strain hardening capacity. The results show that the synergistic effect of strength and ductility can be regulated through lowtemperature short-time annealing with different cryorolling strains, which provides a new reference for the design of future thermo-mechanical processes. 