铸钢粗晶的成因及消除方法的研究

邹安全,邓沛然

中国工程科学 ›› 2005, Vol. 7 ›› Issue (4) : 79 -82.

PDF (5265KB)
中国工程科学 ›› 2005, Vol. 7 ›› Issue (4) : 79 -82.
研究报告

铸钢粗晶的成因及消除方法的研究

作者信息 +

Study on the Formation and Elimination of Coarse Grains in Cast Steel

Author information +
文章历史 +
PDF (5391K)

摘要

通过对ZG32Cr06铸钢粗晶成因的分析及消除粗晶的工艺性能试验,探讨了粗晶导致铸件断裂的机理。试验证明,由于浇铸温度过高,水爆清砂时开箱过早而产生的粗晶可以用热处理方法消除,同时提出了铸件在浇铸时防止粗晶的措施。

Abstract

The relation between coarse grain and rupture of casts was found through analyzing the formation of coarse grains and tests for eliminating coarse grains on ZG32Cr06 cast steel. The results of tests show that the coarse grains, as a results of too high casting temperature and the premature trunk opening in water explosion blast cleaning , can be eliminated by heat treatment. The measures for preventing coarse grains in casts were proposed.

关键词

铸钢 / 粗晶 / 水爆清砂 / 消除方法

Key words

cast steel / coarse grain / water explosion blast cleaning / measures of elimination

引用本文

引用格式 ▾
邹安全,邓沛然 铸钢粗晶的成因及消除方法的研究[J]. 中国工程科学, 2005, 7(4): 79-82 DOI:

登录浏览全文

4963

注册一个新账户 忘记密码

参考文献

AI Summary AI Mindmap
PDF (5265KB)

30

访问

0

被引

详细

导航
相关文章

AI思维导图

/